Advisory Hotline:0371-88817899轉801-808

Portland Cement Refractory Burning Aid And Slag Mud Refractory

Application:

castable Items/Index Portland cement refractory castable Slag cement refractory castable Bulk density (110℃5℃24h) Kg/m3 1900~2100 1900~2100 Drying compressive strength MPa 20 15 Drying strength MPa 4 4 % 30~35 25~30 Thermal shock stabil
Share With:
  • Introduction
  • Application
castable

Items/Index Portland cement
refractory castable
Slag cement refractory
castable
Bulk density
(110℃±5℃×24h)
Kg/m3 1900~2100 1900~2100
Drying compressive
strength
MPa ≥20 15
Drying strength MPa ≥4 4
  % 30~35 25~30
Thermal shock
stability
15 10
After the burning, the
line changes, the
temperature is kept for
3 hours, and the test
temperature is not more than 1%.
1000 900
Refactory 1610 1580
Al2O3 30~40 30~40
Refractory aggregate
maximum particle size
mm - -

castable Items/Index Portland cement refractory castable Slag cement refractory castable Bulk density (110℃5℃24h) Kg/m3 1900~2100 1900~2100 Drying compressive strength MPa 20 15 Drying strength MPa 4 4 % 30~35 25~30 Thermal shock stabil